http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
Jian-Shian Lin,Ming-Hua Chung,Chen-Ming Chen,Fuh-Shyang Juang,Yu-Sheng Tsai,Shu-Wei Chang,Shun-Hsi Wang,Teh-Chao Liao,Lung-Chang Liu 한국물리학회 2010 Current Applied Physics Vol.10 No.5
UV-curable organic/inorganic hybrid composites with gas barrier and heat-dissipating capability have been successfully fast synthesized with microwave irradiation and utilized for the encapsulation of top-emitting organic light-emitting diodes (TEOLEDs). Experimental results manifest that lab-made organic/inorganic hybrid composites can effectively not only obstruct the invasion of moisture as well as oxygen in the atmosphere into the device but also lower the temperature of device. Therefore, the lifetimes of TEOLEDs with their encapsulation are 2.2 folds longer than those without encapsulation.
Jian-Zhe Huang,Li-Hung Lin,Chin-An Chang,Chi-Te Liang,Kuang Yao Chen,Kui-Ming Chen,N. C. Chen,P. H. Chang,Shiou-Shian Han,Zhi-Hao Sun 한국물리학회 2007 THE JOURNAL OF THE KOREAN PHYSICAL SOCIETY Vol.50 No.3
We report on experimental studies of an Al$_{0.15}$Ga$_{0.85}$N/GaN high-electron-mobility transistor structure grown on a $p$-type Si (111) substrate. This structure is compatible with complementary metal-oxide-semiconductor (CMOS) technology and, thus, has great potential device applications. The low-temperature magnetoresistivity shows a parabolic dependence on the applied perpendicular magnetic field. This effect is ascribed to electron-electron interaction (EEI) effects in a weakly-disordered two-dimensional system. Our experimental results agree with the EEI theory when the correction term in the ballistic region has been subtracted.
Shang-Hui Yang,Jian-Shian Lin,Fuh-Shyang Juang,Ding-Chin Chou,Ming-Hua Chung,Chen-Ming Chen,Lung-Chang Liu 한국물리학회 2013 Current Applied Physics Vol.13 No.5
In this paper, white light emitting diodes (LEDs) with good color rendering indices (CRI) and high luminous efficiencies have been fabricated by the encapsulation of mixed and double-deck phosphors. Experimental results revealed that white LEDs with the encapsulation of double-deck phosphors exhibited better CRI and higher luminous efficiencies than those with the encapsulation of mixed phosphors because no secondary excitation took place. The hue, CRI, and luminous efficiencies of white LEDs with double-deck phosphors under 200 mA were CIEx,y =(0.357, 0.348), 90, and 62.3 lm/W,respectively while the hue, CRI, and luminous efficiencies of white LEDs with mixed phosphors under 200 mA were CIEx,y = (0.366, 0.354), 89, and 56.5 lm/W, respectively.
Adjusting optical resonance thickness to increase the conversion efficiency of polymer solar cells
Yu Sheng Tsai,Jian-Shian Lin,Wei-Ping Chu,Po-Hsun Wang,Fuh-Shyang Juang,Ming-Hua Chung,Chin-Ming Chen,Mark O. Liu 한국물리학회 2010 Current Applied Physics Vol.10 No.3
The derivatives of C60, [6,6]-phenyl C61-butyric acid methyl ester (PCBM), and 3-hexylthiophene (P3HT)were dissolved in DCB solvent, then spin coated into an active layer for polymer solar cells. The experimental parameters were studied carefully to obtain the optimum power conversion efficiency (PCE). The primary process for generation of photocurrent in an organic photovoltaic device is the generation of bound electron–hole pairs (excitons) by absorption of energy (photons) from the optical electric field. Modeling was based on the assumption that the photocurrent generation process is the result of the creation and diffusion of photogenerated species (excitons), which are dissociated by charge transfer at the active layer. Improve organic optics absorb by insert organic layer (CuPc or C60) at the active layer/Al interface. This research is divided into two components. First part, we use n-type C60 as transmission layer. When an optimum thickness of C60 is 5 nm, the Jsc of polymer solar cell can be increased from 7.26 mA/㎠ to 7.7 mA/㎠. The Voc decrease is because the energy level of C60 LUMO (lowest unoccupied molecular orbital) at 4.5 eV is higher than the 3.7 eV of PCBM. Second part, we use p-type CuPc as transmission layer. When an optimum thickness of CuPc is 3 nm, the short circuit photo-current density (Jsc) and open circuit voltage (Voc) of polymer solar cell can be increased from 7.26 mA/㎠ to 8.0 mA/㎠ and 0.56–0.58 V, respectively. The reason is the same as C60. The Voc increase is because the energy level of CuPc LUMO (lowest unoccupied molecular orbital) at 3.1 eV is lower than the 3.7 eV of PCBM. The Jsc increase is because the 3 nm of CuPc leads to a constructive interference happened in the active layer and thus optical absorption increases. In this study we used 3 nm of CuPc at the active layer/Al interface to enhance the short circuit current density, and the efficiency was increased to 2.94%.