이동철,김택기,임동묵 대한금속재료학회(대한금속학회) 1989 대한금속·재료학회지 Vol.27 No.4
Thin film of 18,20 and 25at%Ni-Co were prepared by vacuum evaporation technique. The composition and structure of the film and the resulting magnetic properties such as saturation magnetization, magnetic anisotropy and coercive force, have been studied systematically. The microstructure of the films is a mixture of hcp and fcc phases. The saturation magnetization and coefficients of magnetic anisotropy K_(2θ) and K_(46) decr ease with Ni content, while the coercive force increases. The easy axis of magnetization of thin films is parallel to the surface of films. The coercive force strongly depends on the thickness of films, and reaches maximum value at the thickness of about 0.18㎛. The coercive force increases when the films are held at 300℃ for an hour. However, the saturation magnetization is not changed by the heat treatment.
이복희,이국중,전덕규,백승권,임동묵 한국전기전자재료학회 1993 電氣電子材料學會誌 Vol.6 No.3
본 논문은 과도고전압 측정시스템의 단위계단응답으로부터 구한 보정계수를 사용하여 수치계산에 의해 출력값을 보정하는 방법에 대하여 기술하였다. 또한 실규모 용량성분압기의 분압비와 상승시간을 갖는 모의등가회로를 구성하여 측정한 바, 본 연구에서 제안된 보정방법은 급준파 및 차단파 등의 어떠한 입력에도 유용하게 사용할 수 있다.
Alnico 5 의 열처리에 따른 2 상분리조직과 자기특성
김택기,김윤배,송세안,임동묵 대한금속재료학회(대한금속학회) 1986 대한금속·재료학회지 Vol.24 No.5
In order to study a relation between microstructures and magnetic properties in Alnico 5, Fe-24Co-14Ni-8Al-3Cu alloy was prepared by induction melting, and then optimum heat treatment procedures and microstructures of this alloy were investigated systematically. In Alnico 5, the cooling rate(c) in a magnetic field from 900℃ to 600℃ and the optimum aging time(t) at 600℃ have a relation of log(t)=0.417 log(c) + 0.884. However, the final magnetic properties are highly dependent on the cooling rate. Spinodally decomposed structures of this alloy show that the faster the cooling rate, the smaller the size of the FeCo-rich precipitates and the larger the aspect ratio. Length of the long axis of the FeCo-rich precipitates at a given cooling rate is not uniform due to the interconnection of sub sequent precipitates by magnetic field effect, and this tendency seems to be stronger when the cooling rate is slower. But the length of the short axis of the precipitates is almost same at a given cooling rate. The length of the short axis (ℓ) and cooling rate (c) in magnetic field have a relation of log (ℓ)=2.385-0.317 log(c) Optimum solution treatment temperature of the low temperature solution treatment method is 860℃. It is concluded that the low temperature solution treatment method is more desirable than the high temperature solution treatment method in improving the hard magnetic properties
이복희,백용현,박형기,하성철,최창준,임동묵 한국전기전자재료학회 1992 電氣電子材料學會誌 Vol.5 No.4
본 논문은 단로기의 조작 또는 전력기기의 고장시에 흐르는 급준성 대전류에 의하여 발생하는 자계의 측정이 가능한 새로운 센서의 개발에 대하여 기술한다. 동축케이블을 이용한 자기적분형 자계센서의 동작원리 및 설계방법 등에 대하여 이론적으로 해석하고 인가된 자계에 대한 센서응답을 정확하게 결정할 수 있는 교정실험을 수행하였다. 또한 센서의 동작원리에 상응하는 이론적 모델을 제안하였다. 시제작된 자계센서는 적분저항의 증가와 더불어 감지전압이 상승하고 감쇠시간은 줄어드는 특성을 나타내었다. 과도대전류에 의하여 유발되는 방사자계는 거리의 제곱에 반비례하는 특성을 보였으며 전자기기의 보호를 위한 전자차폐장치의 설계시 방사자계성분에 대한 영향을 고려하여야 됨을 확인하였다.