        Synthesis of thin diamond films from faceted nanosized crystallites

        Sobia Allah Rakha,Shumin Yang,Zhoutong He,Ishaq Ahmed,Dezhang Zhu,Jinlong Gong 한국물리학회 2009 Current Applied Physics Vol.9 No.3

        Diamond films consist of crystallites having nanometer grains were deposited using low methane concentration by hot filament chemical vapor deposition (HFCVD). The results show that films consist of nanodiamond grains with grain sizes ranging from 20 nm to 200 nm having thickness dependent size. Increasing the deposition time, the grain size increases and hence the hickness of the film increases. The diamond nucleation (nucleation density 1010 cm-2) is comparable to that obtained by biasing the substrate. The use of low methane concentration for the formation of nano crystallites improves the quality of the film as indicated by Raman spectroscopy. The distance between the filament and substrate is increased while maintaining the substrate temperature. The effects of this large separation on the gas phase chemistry are discussed which helps to understand the reduced size of the crystallites under input gas ratios when microcrystallines are obtained. Diamond films consist of crystallites having nanometer grains were deposited using low methane concentration by hot filament chemical vapor deposition (HFCVD). The results show that films consist of nanodiamond grains with grain sizes ranging from 20 nm to 200 nm having thickness dependent size. Increasing the deposition time, the grain size increases and hence the hickness of the film increases. The diamond nucleation (nucleation density 1010 cm-2) is comparable to that obtained by biasing the substrate. The use of low methane concentration for the formation of nano crystallites improves the quality of the film as indicated by Raman spectroscopy. The distance between the filament and substrate is increased while maintaining the substrate temperature. The effects of this large separation on the gas phase chemistry are discussed which helps to understand the reduced size of the crystallites under input gas ratios when microcrystallines are obtained.