졸-겔 방법으로 제조한 ZnO 쇼트키 다이오드의 특성 연구
한광준(Kwangjoon Han),강광선(Kwangsun Kang),김재환(jaehwan Kim) 대한기계학회 2008 대한기계학회 춘추학술대회 Vol.2008 No.11
ZnO thin films with preferred orientation along the (0 0 2) plane were fabricated by a sol-gel method. The effects of the annealing temperature, time, and thickness were studied by investigating UV-visible spectra, FT-IR spectra, and XRD of ZnO films. The films were dried and annealed at 100 ℃, 200 ℃, and 300 ℃ for 1hr, 2hrs, and 3hrs, respectively. The film showed the preferred (0 0 2) orientation and high transmittance near 90% in the visible range. Also, SEM images of the films exhibited very smooth surfaces without holes and cracks. Schottky diodes were fabricated by using ZnO sol-gel material. Au and Al were used as electrodes to make Ohmic and Schottky contacts, respectively. The annealing temperature, time and the thickness dependent I-V characteristics were presented in this article.