레이저 어블레이션에 의한 $(Pb,La)TiO_3$ 박막의 제작
박정흠,김준한,이상렬,박종우,박창엽,Park, Jeong-Heum,Kim, Joon-Han,Lee, Sang-Yeol,Park, Chong-Woo,Park, Chang-Yub 한국전기전자재료학회 1998 전기전자재료학회논문지 Vol.11 No.2
$(Pb_{0.72}La_{0.28})Ti_{0.93}O_3(PLT(28))$ thin films were fabricated by pulsed laser deposition. PLT films deposited on $Pt/Ti/SiO_2/Si$ at $600^{\circ}C$ had a preferred orientation in (111) plane and at $550^{\circ}C$ had a (100) preferred orientation. We found that (111) preferred oriented films had well grown normal to substrate surface. This PLT(28) thin films of $1{\mu}m$ thickness had dielectric properties of ${\varepsilon}_r$=1300, dielectric $loss{\fallingdotseq}0.03 $. and had charge storage density of 10 [${\mu}C/cm^2$] and leakage current density of less than $10^{-6}[A/cm^2]$ at 100[kV/cm]. These results indicated that the PLT(28) thin films fabricated by pulsed laser deposition are suitable for DRAM capacitor application.