RISS 학술연구정보서비스

검색
다국어 입력

http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.

변환된 중국어를 복사하여 사용하시면 됩니다.

예시)
  • 中文 을 입력하시려면 zhongwen을 입력하시고 space를누르시면됩니다.
  • 北京 을 입력하시려면 beijing을 입력하시고 space를 누르시면 됩니다.
닫기
    인기검색어 순위 펼치기

    RISS 인기검색어

      검색결과 좁혀 보기

      선택해제
      • 좁혀본 항목 보기순서

        • 원문유무
        • 원문제공처
        • 등재정보
        • 학술지명
          펼치기
        • 주제분류
        • 발행연도
          펼치기
        • 작성언어
        • 저자
          펼치기

      오늘 본 자료

      • 오늘 본 자료가 없습니다.
      더보기
      • 무료
      • 기관 내 무료
      • 유료
      • 鋼管圓周溶接部의 溶接殘留應力 分布에 對한 考察

        權鍾完 慶北工業專門大學 1984 論文集 Vol.21 No.-

        Stress due to circumferential V-butt welds, made with six passes in 150mm O.D., 10mm wall thickness cylindrical Cr-Mo alloy pipe, were determined by Sachs boring-out method. The effect of residual stress relief procedures upon to magnitude of stresses and distributions in weld, were investigated. 1. The axial stresses in the weld were founded to be tensile at the innersurface and compressive at the outersurface with maximum compressive stress occurring a short distance below the outersusface. 2. The effect of residual relief stresses, residual stress distributions are same but magnitude is very small by low yielding strength, analyzing time and relaxation of creep. 3. The hardness of welding line were investigated. The stress relief procedures upon to value of hardness is less then received welding. Resulting, magnitude of residual stresses in annealing pipe were founded small value.

      • 變分法에 衣한 體積一定下의 形狀決定에 對한 考察

        權鍾完 慶北工業專門大學 1983 論文集 Vol.20 No.-

        It is very important for structure analysis from the viewpoint of structurl design to know the appropriate shape of beam element. In this paper, The variational approach is formulated in two demensional isotropic plane stress problem and calculate the appropriate shape of element. An example problem, the calcuiation of thickness is showen for simple beam element under the concentrate load. In this study, following information is obtained. 1) An optimal shape condition is expressed by the term fo energy density quantity from principle of variation and example calculation coincides with the solution of uniform stress. 2) we presume the example calculation which is applied more compricate shape calculation problem.

      • 광 간섭법에 의한 계면균열 선단 주위의 개구변위 측정

        權種完,崔柄善 경일대학교 2001 論文集 Vol.17 No.-

        In order to examine near tip asymptotics, it was necessary to make measurements in the crack front region in addition to the globally applied displacements and their associated reactions. Crack opening interferometry, which can measure the normal carck opening displacements directly. A monochromatic beam of light was introduced to the crack faces through beam splitter in the microscope and a 45 degree mirror in the grips. The incident beam was reflected by the crack faces and the reflected beams interfered to form fringe patterns. The fringe patterns from the microscope were recorded through a video camera and timer onto a high resolution video cassette recoder for later determination and analysis of the crack opening profile. The recordings were analyzed using a digital image analysis system to capture, digitize, and store light intensity profiles along the center of the specimen. The whole fringe locating and counting procedure was post-processed so that NCOD profiles could be obtained.

      • 三相스테인리스鋼의 溶體化處理溫度에 對한 靜的强度特性

        權鍾完 慶一大學校 1988 論文集 Vol.4 No.1

        Charactristics of static strength in duplex-stainless steel has been investigated withtemperature of solution heat treatment. In higher temperature, volume of ferrite phase and grain size increased in stainless-steel. At 1623 K, duplex-stainless steel is changed ferrite phase wholy. Static strength and hardness is proportion to volume of ferrite phase. At 1300K, static strength, ductilenss increased significantly. Increasing of cooling rate decreased static strength. The static strength revealed a very large influence of solution temperature at 773K.

      • 2상계 스테인리스강 용접부의 피로크랙 전파특성 (II) -하한계치 근접에서의 전파특성-

        권종완,김상대,이택순 대한기계학회 1989 대한기계학회논문집 Vol.13 No.1

        본 연구에서는 2상계 스테인리스강의 모재,용접재 및 용접후 열처리재 3종류의 경우에 대하여 피로크랙 전파특성을 피로크랙의 하한계치 근방에서 금속조직적인 영향을 검토하기 위하여, 각 조건에 대한 피로크랙 전파속도의 하한 계치를 구하였고 피로식검후의 파단면을 주사전자현미경(SEM)으로 관찰하였다. 용접재에 대하여는 용착부 부근 용접열영향부의 입경측정, .alpha./.gamma.상의 체적비교율의 변화량 측정 및 용접재와 용접후열처리재의 잔유응력분포측정을 통하여 피로크랙의 하한계특성에 미치는 여러가지 영향인자에 대하여 검토하였다. Near-threshold fatigue crack-growth behavior at room temperature for a duplex stainless steel weldments was investigated to evaluate the effect of load ratio, microstructural change, and residual stresses. Near-threshold fatigue crack propagation behavior is found to show a marked sensitivity to .alpha./.gamma. phase ratio, and little residual stress effects. Threshold values in the heat affected zones are higher than those of base metals and threshold values for crack growth decrease with increasing the load ratio in the base metals and weldments. The fractrographic features in base metals, weldments and heat affectred zones were discussed in terms mechanism of crack growth.

      • 워엄 齒東의 齒面摩耗에 對한 考察

        權鍾完 慶北工業專門大學 1980 論文集 Vol.17 No.-

        A worm and worm gear are used to connect nonparallel, shafts and the gear reduction is generally quite large. But worm and worm gear have very large slip ratio on the tooth surface. It is one of important factor that they has different direction between component of contact line and normal velocity. In this paper, the author has considered a relation of contact angle (?) and wear value on the tooth surface. The expriment are carried out cylinder and circular plate in lubricant condition. Exprimental results are as follows; 1) The wear value of contact angle ?=-30˚is twice that of ?=90˚ 2) The wear value is highest at contact angle (?) about 6˚ any other point.

      • 二相 스테인리스鋼 熔接部의 疲勞龜裂傳播 特性과 微視的 機構

        權鍾完 慶一大學校 1989 論文集 Vol.5 No.1

        An experimental study was carried out to identify the fatigue crack propagation behavior of duplex stainless steel weldment. Experimental works were performed under stable crack propagation in room temperature and substitute ocean water was also studied. Experiments were studied to give insight of phenomennological understanding in terms of micro-structural changes. The crack propagation behavior was found to be dependent on phase ratio(α/γ). The crack propagation rate in welding zone first, in base-metal was second. The crack propagation rate in substitute ocean water was found to be faster than that obtained in air at room temperature. This may be caused by the corrosion of the fatigue fracture surface through chemical reaction. The crack propagation rate estimated by the measurement of striation spacing was higher than that obtained by crack length measurement in low △K region, however, both crack propagation rates were found to be identical.

      • 지연 담금질 열처리한 티타늄 합금의 균열 발생과 진전 특성에 관한 연구

        權鍾完 慶一大學校 1996 論文集 Vol.13 No.2

        This study was examined the microstructural parameters which influence the development and growth of short fatigue cracks in the Ti alloy with a view to improving the fatigue performance of the alloy by microstructural control and optimization. The short and long crack growth data has been generated for fully transformed beta and alpha plus transformed beta microstructures containing primary alpha phase volume fractions of 5, 15 and 2% and with prior beta phase grain sizes ranging from approximately 40㎛ up to 1.0㎜. The microstructural features associated with crack initiation and crack propagation have been identified and a simple empirical model has been developed allowing the prediction of fatigue crack growth rates at crack length both above and below the short to long crack transition. In the study have been extended in an attempt to as certain the effects of alpha phase morphology and distribution on the growth of both long and short fatigue cracks in dual phase microstructures. In addition, provisional in-situ SEM observations relating to crack path morphology and the development of crack closure in a 15% alpha microstructures are discussed and an attempt is made to develop a unified approach to fatigue life prediction.

      • 鑄鐵 미끄럼摩擦의 摩耗에 對한 硏究

        權鍾完 慶北工業專門大學 1979 論文集 Vol.16 No.-

        Wear which occurs in the slidng of metal pair is very complicated. Because it is made up the various factors which are combined in a complicated way. In this paper, the relation between wear occurs in matal pair which had been proved depend mainly on the flow pressure of material and Holm's wear equation W=KPL/?? examined by wear test of cast iron. The wear test are carried out under the dry condition using upper and lower test pieces of cast iron the same quality. We proved that material hardness dominated surface temperature induced by frictional temperature. By expressing the hardness as a function of Olad and sliding speed. Results are summarized as follows. 1) ?? could be obtained theoretically from Holm's equation, W=KPL/?? where ?? is wear rate P the load V. the sliding speed. ?? : the hardness at room temperature. C constant depending on the properties of material ?? : flow pressure. 2) The equation did not hold at high load and speed, this cause is deduced that some factors other than the hardness act predominantly on the wear process.

      • 2相 Stainless鋼의 異種熔接에 對한 靜的 强度特性

        權鍾完 慶一大學校 1986 論文集 Vol.2 No.1

        Recent trends in the fabrication of industrial plant have led to the increased use of welding for joining materials of different composition. In this study, is research of static strength for welding bond by dissimilar metals(25cr-5Ni stainless steel versus SM41 steel). Through investigation, we found phenomenon of maxium true strength and toughness decreasing near the bonded part of welding joint. It was caused by brittle layer formed in the deposite metal along the fusion line. We recognized accurate time for PWHT(post welding heat treatment 1hr or 2hr.) Brittle layer of welding bond is recovered by PWHT in this case.