Oxidation Behavior of (W, Re)-Bearing Single Crystal Nickel-Base Superalloys
Junhee Hahn,Dongyi Seo,Sunghun Lee,Eungseon Byon,Dong Bok Lee 대한금속·재료학회 2021 METALS AND MATERIALS International Vol.27 No.8
Four kinds of single-crystal Ni-base superalloys (12Ta–7.5Cr–5Co–4.8Al–1.9Mo–1Ti, balance Ni in wt%) containing (0–3)wt%W and (1–4) wt%Re were cast, and oxidized at 1000 °C for up to 275 h in air. In the as-cast condition, the microsegregations of (Cr, Co, Mo, W, Re) in the dendrites and (Al, Ti, Ta) in the interdendritic regions were observed. The γ/γ′ eutecticphases formed in the interdendritic regions. The oxidation rate of the cast alloys was comparable to that of the 2nd generation alloys, displaying relatively good oxidation resistance due primarily to the formation of stable alumina and chromia onthe surface. Especially, the alloy with 2 wt% W and 2 wt% Re showed the best oxidation resistance among the four alloys. Uniform oxidation occurred in the dendrite area, whereas nodular oxidation occurred in the interdendrite region.