RISS 학술연구정보서비스

검색
다국어 입력

http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.

변환된 중국어를 복사하여 사용하시면 됩니다.

예시)
  • 中文 을 입력하시려면 zhongwen을 입력하시고 space를누르시면됩니다.
  • 北京 을 입력하시려면 beijing을 입력하시고 space를 누르시면 됩니다.
닫기
    인기검색어 순위 펼치기

    RISS 인기검색어

      검색결과 좁혀 보기

      선택해제

      오늘 본 자료

      • 오늘 본 자료가 없습니다.
      더보기
      • 무료
      • 기관 내 무료
      • 유료
      • SCIESCOPUSKCI등재

        The effect of repeated firings on the color change of dental ceramics using different glazing methods

        Yilmaz, Kerem,Gonuldas, Fehmi,Ozturk, Caner The Korean Academy of Prosthodonitics 2014 The Journal of Advanced Prosthodontics Vol.6 No.6

        PURPOSE. Surface color is one of the main criteria to obtain an ideal esthetic. Many factors such as the type of the material, surface specifications, number of firings, firing temperature and thickness of the porcelain are all important to provide an unchanged surface color in dental ceramics. The aim of this study was to evaluate the color changes in dental ceramics according to the material type and glazing methods, during the multiple firings. MATERIALS AND METHODS. Three different types of dental ceramics (IPS Classical metal ceramic, Empress Esthetic and Empress 2 ceramics) were used in the study. Porcelains were evaluated under five main groups according to glaze and natural glaze methods. Color changes (${\Delta}E$) and changes in color parameters (${\Delta}L$, ${\Delta}a$, ${\Delta}b$) were determined using colorimeter during the control, the first, third, fifth, and seventh firings. The statistical analysis of the results was performed using ANOVA and Tukey test. RESULTS. The color changes which occurred upon material-method-firing interaction were statistically significant (P<.05). ${\Delta}E$, ${\Delta}L$, ${\Delta}a$ and ${\Delta}b$ values also demonstrated a negative trend. The MC-G group was less affected in terms of color changes compared to other groups. In all-ceramic specimens, the surface color was significantly affected by multiple firings. CONCLUSION. Firing detrimentally affected the structure of the porcelain surface and hence caused fading of the color and prominence of yellow and red characters. Compressible all-ceramics were remarkably affected by repeated firings due to their crystalline structure.

      • KCI등재

        The effect of repeated firings on the color change and surface roughness of dental ceramics

        Caner Ozturk,Kerem Yılmaz,Fehmi Gonuldas 대한치과보철학회 2014 The Journal of Advanced Prosthodontics Vol.6 No.4

        PURPOSE The color of the ceramic restorations is affected by various factors such as brand, thickness of the layered the ceramic, condensation techniques, smoothness of surface, number of firings, firing temperature and thickness of dentin. The aim of this study was to evaluate the color change and surface roughness in dental porcelain with different thicknesses during repeated firings. MATERIALS AND METHODS Disc-shaped (N=21) metal-ceramic samples (IPS Classic; Ivoclar Vivadent; Shaar, Liechtenstein) with different thickness were exposed to repeated firings. Color measurement of the samples was made using a colorimeter and profilometer was used to determine surface roughness. ANOVA and Tukey tests with repeated measurements were used for statistical analysis. RESULTS The total thickness of the ceramics which is less than 2 mm significantly have detrimental effect on the surface properties and color of porcelains during firings (P<.05). CONCLUSION Repeated firings have effects on the color change and surface roughness of the dental ceramics and should be avoided.

      • SCIESCOPUSKCI등재

        The effect of repeated firings on the color change of dental ceramics using different glazing methods

        Caner Ozturk,Fehmi Gonuldas,Kerem Yılmaz 대한치과보철학회 2014 The Journal of Advanced Prosthodontics Vol.6 No.6

        PURPOSE Surface color is one of the main criteria to obtain an ideal esthetic. Many factors such as the type of the material, surface specifications, number of firings, firing temperature and thickness of the porcelain are all important to provide an unchanged surface color in dental ceramics. The aim of this study was to evaluate the color changes in dental ceramics according to the material type and glazing methods, during the multiple firings. MATERIALS AND METHODS Three different types of dental ceramics (IPS Classical metal ceramic, Empress Esthetic and Empress 2 ceramics) were used in the study. Porcelains were evaluated under five main groups according to glaze and natural glaze methods. Color changes (ΔE) and changes in color parameters (ΔL, Δa, Δb) were determined using colorimeter during the control, the first, third, fifth, and seventh firings. The statistical analysis of the results was performed using ANOVA and Tukey test. RESULTS The color changes which occurred upon material-method-firing interaction were statistically significant (P<.05). ΔE, ΔL, Δa and Δb values also demonstrated a negative trend. The MC-G group was less affected in terms of color changes compared to other groups. In all-ceramic specimens, the surface color was significantly affected by multiple firings. CONCLUSION Firing detrimentally affected the structure of the porcelain surface and hence caused fading of the color and prominence of yellow and red characters. Compressible all-ceramics were remarkably affected by repeated firings due to their crystalline structure.

      • SCIESCOPUSKCI등재

        The effect of repeated firings on the color change and surface roughness of dental ceramics

        Gonuldas, Fehmi,Yilmaz, Kerem,Ozturk, Caner The Korean Academy of Prosthodonitics 2014 The Journal of Advanced Prosthodontics Vol.6 No.4

        PURPOSE. The color of the ceramic restorations is affected by various factors such as brand, thickness of the layered the ceramic, condensation techniques, smoothness of surface, number of firings, firing temperature and thickness of dentin. The aim of this study was to evaluate the color change and surface roughness in dental porcelain with different thicknesses during repeated firings. MATERIALS AND METHODS. Disc-shaped (N=21) metal-ceramic samples (IPS Classic; Ivoclar Vivadent; Shaar, Liechtenstein) with different thickness were exposed to repeated firings. Color measurement of the samples was made using a colorimeter and profilometer was used to determine surface roughness. ANOVA and Tukey tests with repeated measurements were used for statistical analysis. RESULTS. The total thickness of the ceramics which is less than 2 mm significantly have detrimental effect on the surface properties and color of porcelains during firings (P<.05). CONCLUSION. Repeated firings have effects on the color change and surface roughness of the dental ceramics and should be avoided.

      • KCI등재

        Electromyography-Guided Botulinum Toxin Injection Into the Cricothyroid Muscles in Bilateral Vocal Fold Abductor Paralysis

        Mustafa Sahin,Ibrahim Aydogdu,Serdar Akyildiz,Munevver Erdinc,Kerem Ozturk,Fatih Ogut 대한이비인후과학회 2017 Clinical and Experimental Otorhinolaryngology Vol.10 No.2

        Objectives. Bilateral vocal fold abductor paralysis (BVFAP) both deteriorates quality of life and may cause life-threatening respiratory problems. The aim of this study was to reduce respiratory symptoms in BVFAP patients using cricothyroid (CT) botulinum toxin (BTX) injection. Methods. Before and 2 weeks and 4 months after bilateral BTX injection into the CT muscles under electromyography; alterations in respiratory, acoustic, aerodynamic and quality of life parameters were evaluated in BVFAP patients with respiratory distress. For the respiratory evaluation modified Borg scale and spirometry, for the voice and aerodynamic evaluations Voice Handicap Index-30 (VHI-30), GRBAS, acoustic analysis (sound pressure level, F0, jitter%, shimmer%, noise-to-harmonic ratio) and maximum phonation time and for the quality of life assessment Short Form-36 (SF-36) form were used. Results. All patients were female with a mean age of 47±8.1 years. There was a mean time of 11.8±5.5 (minimum 2, maximum 23) months between BVFAP development and BTX injection. In all cases, other than one case with unknown aetiology, the cause of vocal fold paralysis was prior thyroid surgery. In total 18.6±3.1 units of BTX were applied to the CTs. In the preinjection period, and the 2nd week and 4th month after injection, the Borg dyspnea scale was 7.3/5.3/5.0, FIV1 (forced inspiratory volume in one second) was 1.7/1.7/1.8 L, peak expiratory flow (PEF) was 1.4/1.7/2.1 L/sec, maximum phonation time was 7.0/6.4/6.2 seconds and VHI-30 was 63.2/52.2/61.7 respectively. There was no significant alteration in acoustic analysis parameters. Many of the patients reported transient dysphagia within the first week. There were insignificant increases in SF-36 sub-scale values. Conclusion. After BTX injection, improvements in the mean Borg score, PEF and FIV1 values and SF-36 sub-scale scores showed the restricted success of this approach. This modality may be kept in mind as a transient treatment option for patients refused persistent tracheotomy or ablative airway surgeries.