        Effect of Y2O3 content on Ni60 alloy cladding layer

        Fangping Yao,Zhi Ming,Jinhua LI,Xiang Chen 대한기계학회 2022 JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY Vol.36 No.9

        Six kinds of Ni60 alloy coatings with different percentage of Y 2 O 3 were prepared by laser cladding. A metallurgical microscope was used to analyze the morphology of the cladding layer. Scanning electron microscopy and EDS energy spectrum analysis were used to characterize the microstructure and element segregation of the cladding layer. A Vickers microhardness tester was used to measure the hardness of the cladding layer. Finally, a friction and wear tester established the friction and wear properties of the cladding layer. The study results show that Y 2 O 3 can significantly reduce the height of the cladding layer and increase the width of the cladding layer; it can also improve the structure refinement and element segregation of the cladding layer. The microhardness of the cladding layer is significantly improved compared to the Ni60 alloy coating without Y 2 O 3 , thereby enhancing the wear resistance of the coating.

      • KCI등재

        Simulation of in-situ preheating of ni-based multi-layer and multi-pass coatings on H13 steel

        Honggang Yin,Jinhua LI,Liwei Zhao,Fangping Yao 대한기계학회 2022 JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY Vol.36 No.9

        COMSOL was used to simulate the temperature field of the preheating and nonpreheating processes of the laser cladding multi-layer and multi-pass coating, and experimental verification was carried out. The results show that the temperature gradient value of the coating at the Z-axis is much larger than the value at the X and Y-axis, respectively. It indicates that the coating is sensitive to cracks at the Z-axis. After preheating, the quality of the coating is improved, and the results of the geometric morphology in experiments are basically consistent with the results of simulation. With increase in coating temperature, the cladding efficiency increased. The difference of temperature between the first and second layer was significantly reduced. The temperature gradient value at the Z-axis decreased. The coating grain structure presents as refined and well-distributed. The temperature gradient size in each layer decreased with the number of coatings increasing.