0.1 M HCl이 포함된 아임계수 및 초임계수 용액에서 Alloy 625의 부식거동
이규환 ( Kyu Hwan Lee ),이무중 ( Moo Joong Lee ),장도연 ( Do Yon Chang ) 대한금속재료학회 ( 구 대한금속학회 ) 2006 대한금속·재료학회지 Vol.44 No.7
Corrosion tests of alloy 625 in subcritical- and supercritical water containing 0.1 M HCI were performed in the range of temperature of 350℃~450℃ at 25 MPa. The corrosion rate of alloy 625 was faster in sub critical water than in supercritical water. 0.1 M of hydrogen peroxide seemed critical concentration of oxidizer that accelerated the corrosion rate of alloy 625. Below 0.1 M of hydrogen peroxide, corrosion rate was not influenced, however, over 0.1 M, corrosion rate was increased rapidly with increasing the hydrogen peroxide. Alloy 625 had two corroded layers. Intermediate layer was the porous structure layer in which Ni and/or Fe were dissolved out selectively. The outer layer was a powder-like porous oxide layer mainly composed with chromium oxide. It was found that the main corrosion mechanisms of alloy 625 were selective dissolution of nickel and iron under the subcritical water and selective dissolution of nickel under the highly oxidized supercritical water condition.