        Preparation of petroleum impregnating pitches from pyrolysis fuel oil using two‑step heat treatments

        Jong‑Eun Choi,Seunghyun Ko,Young‑Pyo Jeon 한국탄소학회 2019 Carbon Letters Vol.29 No.4

        Petroleum-based impregnating pitches were prepared from pyrolysis fuel oil (PFO) using a two-step heat treatment without a separation process. The pressurized heat treatment, the first step, was used to improve the properties of the pitches and enhance the product yield by promoting the cracking and polymerization of the components in the PFO. An atmospheric heat treatment as the second step was used only to synthesize the impregnating pitches from the liquid pitches prepared during the first step. The prepared impregnating pitches had the properties of a commercial petroleum-based impregnating pitch. The impregnation performance was evaluated by HT-XRD and an impregnation test. The HT-XRD results showed changes in the stacked structure of the pitches at the impregnation temperature. The bulk density of the carbon block was increased to 14.3% and the porosity was reduced by 10.3% after the impregnation/recarbonization process. The high reaction temperature during the first step induced the formation of quinoline insoluble (QI) components during the second step of the treatment, and the QI components adversely affected the impregnation process.

      • KCI등재

        Preparation of petroleum impregnating pitches from pyrolysis fuel oil using two-step heat treatments

        최종은,고승현,전영표 한국탄소학회 2019 Carbon Letters Vol.29 No.4

        Petroleum-based impregnating pitches were prepared from pyrolysis fuel oil (PFO) using a two-step heat treatment without a separation process. The pressurized heat treatment, the first step, was used to improve the properties of the pitches and enhance the product yield by promoting the cracking and polymerization of the components in the PFO. An atmospheric heat treatment as the second step was used only to synthesize the impregnating pitches from the liquid pitches prepared during the first step. The prepared impregnating pitches had the properties of a commercial petroleum-based impregnating pitch. The impregnation performance was evaluated by HT-XRD and an impregnation test. The HT-XRD results showed changes in the stacked structure of the pitches at the impregnation temperature. The bulk density of the carbon block was increased to 14.3% and the porosity was reduced by 10.3% after the impregnation/recarbonization process. The high reaction temperature during the first step induced the formation of quinoline insoluble (QI) components during the second step of the treatment, and the QI components adversely affected the impregnation process.