Martin Herrera Trejo,Eddy Alfaro Lopez,Jose Jorge Ruiz Mondragon,Manuel de Jesus Castro Roman,Hugo Solis Tovar 대한금속·재료학회 2010 METALS AND MATERIALS International Vol.16 No.5
The solidification path and contraction generated during the solidification of three carbon steels were studied. Two of the carbon steels were of hypo-peritectic chemical composition, with 0.11 % C and 0.15 % C, while one of the carbon steels were hyper-peritectic with 0.16 % C. The steels with 0.11 % C and 0.16 % C solidified as expected due to their chemical composition. In contrast, the chemically hypo-peritectic steel with 0.15 % C solidified as hyper-peritectic steel, which was associated with the microsegregation of Mn. For the steel exhibiting a hypo-peritectic solidification path, peritectic transformation occurred at solid fraction values higher than 0.9, where it was assumed that the contraction generated in the mushy shell cannot be fed by the liquid. However, for steels exhibiting a hyper-peritectic solidification path, peritectic transformation began at solid fraction values lower than 0.9, where the contraction generated by the peritectic transformation was partly fed by the liquid. Hence, the highest cracking susceptibility was associated with the hypo-peritectic solidification mode.