http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
Sintering and Mechanical Properties of Chromium Boride-chromium Carbide Composites
Matsushita Jun-Ichi,Shimao Kenji,Machida Yoshiyuki,Takao Takumi,Iizumi Kiyokata,Sawada Yutaka,Shim Kwang-Bo 한국분말야금학회 2006 한국분말야금학회 학술대회논문집 Vol.2006 No.1
Several boride sintered bodies such as , , and were previously reported. In the present study, the sinterability and physical properties of chromium boride containing chromium carbide sintered bodies were investigated in order to determine its new advanced material. The samples were sintered at desired temperature for 1 hour in vacuum under a pressure by hot pressing. The relative density of sintered bodies was measured by Archimedes' method. The relative densities of addition of 0, 5, 10, 15 and 20 mass% composites were 92 to 95%. The Vickers hardness of the with 10 and 15 mass% composites were about 14 and 15 GPa at room temperature, respectively. The Vickers hardness at high temperature of the addition of 10 mass% composite decreased with increasing measurement temperature. The Vickers hardness at 1273 K of the sample was 6 GPa. The Vickers hardness of addition of composites was higher than monolithic sintered body. The powder X-ray diffraction analysis detected CrB and phases in containing composites.