        Structural Design and Property Evaluations of Foam-based Composite Materials: Effect of Perforation Depth and Foam Density on the Mechanical, Sound Absorption, and Thermal Properties

        Ruei-Ren Ou,Chen-Hung Huang,Ching-Wen Lou,Jia-Horng Lin 한국섬유공학회 2021 Fibers and polymers Vol.22 No.3

        Nonwoven fabrics and rigid polyurethane foam(PUF) are commonly used materials as building materials, butthere are few studies on combining both materials and reporting characteristic evaluations for the application. In this study, N/L/Fr nonwoven fabrics are combined with PUF to produce N/PUF composites, and then a needle punching machine is usedfor perforation, thereby produces perforated N/PUF composites. With PUF densities being 70 kg/m3 and 80 kg/m3, aperforation depth of 100 % results in significantly decreasing mechanical properties. Based on the results of thermalconductivity coefficient, the employment of needle punch process results in a decrease in the thermal insulation of N/PUFcomposite; however, the descending level is comparatively smaller when PUF is made of a greater density. In thethermogravimetric analysis (TGA), the char residue is 4.86 % for PUF and 11.68 % for N/PUF composites, indicating thatN/L/Fr nonwoven fabrics improve the thermal stability of PUF. As per limiting oxygen index (LOI), the part of proposed N/PUF composites that first contacts the flame is N/L/Fr nonwoven fabrics, which causes an LOI of 33 when in practicalapplication and resembles the LOI (33) of N/L/Fr nonwoven fabrics. Based on the test results, the optimal perforated N/PUFcomposites are made of a PUF density of 80 kg/m3 and a perforation depth of 75 %, and the optimal compression strength is375.29 kPa, which increases by 10.96 %. In addition, the proposed products have the same impact absorption capacity (5.88 J) asthat of N/PUF composites, which absorb a total of 98.16 % impact energy. The sound absorption is improved in the frequencyband of 800-2500 Hz, which broadens the sound absorption bandwidth and benefits the application as being sound absorbentmaterials.