M. I. Pech-Canul,M. Rodríguez-Reyes3,M. A. Pech-Canul,J. C. Rendón-Angeles 대한금속·재료학회 2011 METALS AND MATERIALS International Vol.17 No.6
In this work, SiC_P and SiC_P/SiO_2 porous preforms were infiltrated without assistance in Ar→N_2 atmosphere with the alloy Al-10.3 Mg-12.04 Si (wt.%) at 1050 and 1100 °C, for 20, 40 and 60 min. It was found that a decrease in residual porosity and an increase in elastic modulus by about 22 % with respect to composites produced without SiO_2 additions to the preforms are associated with the formation of magnesium aluminate spinel (MgAl_2O_4). A concurrent increase of the matrix hardness is ascribed to a strengthening mechanism by MgAl_2O_4 formation, similar to the strengthening observed with Mg_2Si in aluminum alloys. Therefore, the spinel can be considered as a co-reinforcement of SiC_p in the aluminum matrix composites. Reactions for spinel formation and possible mechanisms for hardness enhancement are outlined.