Avelar Alan Matias,de Camargo Fábio,da Silva Vanessa Sanches Pereira,Giovedi Claudia,Abe Alfredo,Mourão Marcelo Breda 한국원자력학회 2023 Nuclear Engineering and Technology Vol.55 No.1
This study investigates the high temperature oxidation behaviour of a Nie20Cr-1.2Si (wt.%) alloy in steam from 1200 C to 1350 C by Thermogravimetric Analysis (TGA), Scanning Electron Microscopy (SEM), Energy Dispersive X-ray Spectroscopy (EDS) and X-ray Diffraction (XRD). The results demonstrate that exposed Ni-based alloy developed a thin oxide scale, consisted mainly of Cr2O3. The oxidation kinetics obtained from the experimental results was applied to evaluate the hydrogen generation considering a simplified reactor core model with different cladding alloys following an unmitigated Loss- Of-Coolant Accident (LOCA) scenario in a hypothetical Small Modular Reactor (SMR). Overall, experimental data and simulations results show that both Fe-based and Ni-based alloys may enhance cladding survivability, delaying its melting, as well as reducing hydrogen generation under accident conditions compared to Zr-based alloys. However, a substantial neutron absorption occurs when Ni-based alloys are used as cladding for current uranium-dioxide fuel systems, even when compared to Fe-based alloys.