NH₃가스 미량첨가 분위기에서의 CO-H₂혼합가스에 의한 과탄화철의 합성
정성실,정우창,강흥원,박응열,정원섭,박익민 대한금속재료학회 2004 대한금속·재료학회지 Vol.42 No.11
The synthesis process of iron carbide was proceeded in two stages of reduction of hematite fines by H₂ gas, and carburization of the reduced metal by CO-H₂ gas mixture at 600℃. The surface of reduced iron was pre-treated with an addition of 0.05 vol% NH₃-Ar before carburization. The synthesized iron carbides were comprehensively explored by C/S analyzer (Low C/S determinator), Mossbauer spectroscopy, X-ray diffraction patterns (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and Raman spectroscopy at various reaction times of 5, 10, 15, 20, 25, 30, and 35 min. By addition of a small amount of NH3 gas, the super iron carbides contained 10 wt% carbon were made, and such addition stabilized iron carbides. It was found that addition of NH3 gas played a major role in the formation of iron carbide without decomposition (Fe₃C→ 3Fe+C) of iron carbides and precipitation of free carbon. From these results, we succeed in synthesis of super iron carbide, Fe_(5)C₂, with a stable single phase without Fe and Fe₃C phases. (Received August 2, 2004)