- Abstract
- 1. 서론
- 2. 시험편 및 실험방법
- 2.1 시험편
- 2.2 실험방법
http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
목차 (Table of Contents)
참고문헌 (Reference)
1 박성완, "접착이음의 강도평가에 대한 해석" 한국생산제조시스템학회 14 (14): 62-73, 2005
2 박성완, "인장-비틀림 하중에 의한 섬유강화 복합재료의 피로수명 예측" 한국생산제조시스템학회 13 (13): 64-73, 2004
3 박성완, "연성접착제를 사용한 접착이음의 강도평가에 대한 해석" 한국기계기술학회 11 (11): 23-32, 2009
4 박성완, "경계요소 순차근사법에 의한 응력확대계수 평가" 한국기계기술학회 10 (10): 1-8, 2008
5 L. M. Keer, "The Singularity at the Apex of a Bonded Wedge-Shaped Stamp" 46 : 577-583, 1979
6 H. L. Groth, "Stress Singularities and Fracture at Interface Corners in Bonded Joinats" 8 (8): 107-114, 1988
7 W. S. Johnson, "Stress Analysis of the Cracked-Lap-Shear Specimen" 15 (15): 303-311, 1987
8 A. J. Kinloch, "Stractural Adhesives Developments in Resins and Primers" Elsevier Applied Science Publishers 127-161, 1986
9 J. P. Dempsey, "On the Stress Singularities in the Plate Elasticity of Composite Wedge" 9 (9): 373-382, 1979
10 R. I. Zwiers, "On the Logarithmic Singularity of Free Edge Stress in Laminated Composites under Uniform Expansion" 49 : 561-569, 1982
1 박성완, "접착이음의 강도평가에 대한 해석" 한국생산제조시스템학회 14 (14): 62-73, 2005
2 박성완, "인장-비틀림 하중에 의한 섬유강화 복합재료의 피로수명 예측" 한국생산제조시스템학회 13 (13): 64-73, 2004
3 박성완, "연성접착제를 사용한 접착이음의 강도평가에 대한 해석" 한국기계기술학회 11 (11): 23-32, 2009
4 박성완, "경계요소 순차근사법에 의한 응력확대계수 평가" 한국기계기술학회 10 (10): 1-8, 2008
5 L. M. Keer, "The Singularity at the Apex of a Bonded Wedge-Shaped Stamp" 46 : 577-583, 1979
6 H. L. Groth, "Stress Singularities and Fracture at Interface Corners in Bonded Joinats" 8 (8): 107-114, 1988
7 W. S. Johnson, "Stress Analysis of the Cracked-Lap-Shear Specimen" 15 (15): 303-311, 1987
8 A. J. Kinloch, "Stractural Adhesives Developments in Resins and Primers" Elsevier Applied Science Publishers 127-161, 1986
9 J. P. Dempsey, "On the Stress Singularities in the Plate Elasticity of Composite Wedge" 9 (9): 373-382, 1979
10 R. I. Zwiers, "On the Logarithmic Singularity of Free Edge Stress in Laminated Composites under Uniform Expansion" 49 : 561-569, 1982
11 L. A. Carlsson, "On the Analysis and Design of the End Notched Flexure(ENF)Specimen for Mode Ⅱ" 20 : 594-604, 1986
12 C. Atkinson, "On Stress Singularities and Interface in Liner Elastic Fracture Mechanics" 13 (13): 807-812, 1977
13 박성완, "ModeⅠ 하중에서의 에폭시계 접착제의 피로균열 진전특성" 한국기계기술학회 15 (15): 5-13, 2013
14 L. A. Carlsson, "Mode Ⅱ Interlaminer Fracture of Graphite/Epoxy and Graphite/PEEK" 5 : 170-, 1986
15 K. M. Liechti, "Fracture Testing and Failure Analysis"
16 A. F. Yee, "Fractography and Failure Mechanics of Rubber Modified Epoxy Resigns" Elsevier Apple. Sci.
17 M. Comninou, "Effect of Friction on the Interface Crack Loaded in Shear" 10 (10): 203-210, 1980
18 C. Mall, "Effect of Bond Thickness on Fracture and Fatigue Strength of Adhesively Bonded" 9 (9): 33-37, 1989
19 H. Chai, "Design Aspects of The End-Notch Adhesive Joint Specimen" 36 : R3-R8, 1988
20 H. Zhang, "Deformation and Fracture of Glass Bead/CTBN-Rubber/Epoxy Composites" 33 (33): 10-25, 1993
21 S. O. Park, "A Study for Mutual Interference between Circular Inclusion and Crack in Finite-Width Plate by Boundary Element Method" 18 (18): 1474-1482, 1994
22 P. A. Gradin, "A Fracture Criterion for Edge-Bonded Bimaterial Bodies" 16 : 448-456, 1982
23 P. C. Paris, "A Critical Analysis of Crack Propagation Laws" ASME 85 : 528-534, 1960
24 Penado, F. E, "A Closed Form Solution for the Energy Release Rate of the Double Cantilever Beam Specimen with an Adhesive Layer" 27 (27): 383-407, 1993
태양열 에너지 저장탱크에서의 충진제 특성 및 HTF 유입속도에 따른 열유동 해석
학술지 이력
연월일 | 이력구분 | 이력상세 | 등재구분 |
---|---|---|---|
2026 | 평가예정 | 재인증평가 신청대상 (재인증) | |
2020-01-01 | 평가 | 등재학술지 유지 (재인증) | |
2017-01-01 | 평가 | 등재학술지 유지 (계속평가) | |
2015-04-01 | 학회명변경 | 영문명 : Journal of the Korean Society of Mechanical Technology -> Korean Society of Mechanical Technology | |
2014-01-01 | 평가 | 등재학술지 선정 (계속평가) | |
2013-01-01 | 평가 | 등재후보 1차 PASS (등재후보1차) | |
2012-01-01 | 평가 | 등재후보학술지 유지 (기타) | |
2011-01-01 | 평가 | 등재후보 1차 FAIL (등재후보2차) | |
2010-01-01 | 평가 | 등재후보 1차 PASS (등재후보1차) | |
2008-01-01 | 평가 | 등재후보학술지 선정 (신규평가) |
학술지 인용정보
기준연도 | WOS-KCI 통합IF(2년) | KCIF(2년) | KCIF(3년) |
---|---|---|---|
2016 | 0.4 | 0.4 | 0.36 |
KCIF(4년) | KCIF(5년) | 중심성지수(3년) | 즉시성지수 |
0.39 | 0.38 | 0.279 | 0.22 |