The intension of this study is to produce ordinary portland cement using ash, both bottom ash and fly ash, obtained from municipal solid waste incineration ash (MSWI). We used limestone, waste molding sand, shale, slag from converting furnaces and fly...
The intension of this study is to produce ordinary portland cement using ash, both bottom ash and fly ash, obtained from municipal solid waste incineration ash (MSWI). We used limestone, waste molding sand, shale, slag from converting furnaces and fly ash as main raw materials and mixed them, setting the lime saturation factor (LSF) within 91.0, the silica modulus (SM) within 2.40, and iron modulus (IM) within 1.80. We conducted tests adding bottom ash alone 1, 2 and 3% by weight, respectively, and a mixture of bottom ash 0.9% and fly ash 0.1 % by weight. The result of analysis on clinker shows that the more ash is added, the lower the burnability index (B.I.) falls, lowering the mineral evolution of calcium silicate accordingly. From the measurement of compressive strength we have learned that the more ash is used, the lower the strength becomes.