The pelletizing of printed circuit board (PCB) sludge was researched for copper recovery in pyrometallurgical process. This pelletizing was carried out by using self-manufactured compression-type apparatus after pre-treatments (drying, water scrubbing...
The pelletizing of printed circuit board (PCB) sludge was researched for copper recovery in pyrometallurgical process. This pelletizing was carried out by using self-manufactured compression-type apparatus after pre-treatments (drying, water scrubbing, size classification) were proceeded. The physical properties (compression strength and drop-breakage test) were tested with a change of sludge sizing and the number of compression. In the case of using the undersized sludge of #140, its properties were improved to 0.6 MPa and 9.3 times. Moreover, they increased to 0.82 MPa and 19.0 times by using the #140 ~ 325 sludge. These imply that the packing density increases due to the elimination of large-sized sludge (#140), and also the weight of required binder decreases by the removal of fine-sized sludge (#325).