    시멘트 콘크리트 포장의 구조진단 및 중점보수기법 연구  :  (A Study on the Structural Evaluation and Major Rehabilitation Procedure for Portland Cement Concrete Pavement)

    한글로보기

    https://www.riss.kr/link?id=G3624432

    • 0

      상세조회
    • 0

      다운로드
    서지정보 열기
    • 내보내기
    • 내책장담기
    • 공유하기
      • URL 복사
    • 오류접수
    인용문이 복사되었습니다.

    부가정보

    다국어 초록 (Multilingual Abstract) kakao i 다국어 번역

    For long life cycle and good load capacity, it is increased to use rigid highway pavements. Upon recently research on the defects apparent on JCP, it is reported that joint seal damage is 48%, joint spalling 22%, patching deterioration 15% and transverse crack 6%. In present study, the structural rehabilitation and the expectation of remaning service life of existing pavement are investigated. And also, the fatigue life prediction model on the cutting point of pavement is constructed. The concept of repair method based on priority is presented and falling Weight Deflectometer (FWD) is selected for the measuring equipment of residual life of pavement. Static stress analysis using modified JSLAB and general FEM program are performed in order to examine the effect of temperature and subgrade conditon about behavior of JCP at joint. Also, to study joint spalling and load transfer loss, we performed fatigue test in the laboratory. The specimen was scaled down 1/3 for one lane JCP. Fatigue load was 0.7ton based on 18-kip equivalent single-axle loads. The frequency of loading was five cycles per second.
    번역하기

    For long life cycle and good load capacity, it is increased to use rigid highway pavements. Upon recently research on the defects apparent on JCP, it is reported that joint seal damage is 48%, joint spalling 22%, patching deterioration 15% and transve...

    For long life cycle and good load capacity, it is increased to use rigid highway pavements. Upon recently research on the defects apparent on JCP, it is reported that joint seal damage is 48%, joint spalling 22%, patching deterioration 15% and transverse crack 6%. In present study, the structural rehabilitation and the expectation of remaning service life of existing pavement are investigated. And also, the fatigue life prediction model on the cutting point of pavement is constructed. The concept of repair method based on priority is presented and falling Weight Deflectometer (FWD) is selected for the measuring equipment of residual life of pavement. Static stress analysis using modified JSLAB and general FEM program are performed in order to examine the effect of temperature and subgrade conditon about behavior of JCP at joint. Also, to study joint spalling and load transfer loss, we performed fatigue test in the laboratory. The specimen was scaled down 1/3 for one lane JCP. Fatigue load was 0.7ton based on 18-kip equivalent single-axle loads. The frequency of loading was five cycles per second.

    더보기

    목차 (Table of Contents)

    • 목차
    • 표목차
    • 그림목차
    • 요약
    • 1. 연구목적 및 개요
    • 목차
    • 표목차
    • 그림목차
    • 요약
    • 1. 연구목적 및 개요
    • 1.1 연구목적
    • 1.3 개요
    • 2.구조진단 및 중점보수기법
    • 2.1 포장구조진단기
    • 2.2 NDT(비파괴시험) 포장처짐 측정
    • 3. 줄눈 콘크리트 포장의 피로실험 계획
    • 3.1 개요 및 일반사항
    • 3.2 하중전달(LOAD TRANSFER)과 줄눈부 SPALLING
    • 3.3 줄눈 콘크리트포장의 유한요소 해석
    • 3.4 구조해석 프로그램의 작성
    • 4. 모형슬래브 피로시험 실시 및 결과분석
    • 4.1 모형 줄눈 콘크리트포장 시험체의 설계 및 제작
    • 4.2 모형 줄눈 콘크리트포장의 정적하중 재하실험
    • 4.3 모형 줄눈 콘크리트포장의 피로실험
    • 결론 및 제언
    • 주요참고문헌
    • 부록A 실용화 연구보고서(반강성 포장에 대한 실험적 연구)
    • 부록B 반강성 포장공법 실용화를 위한 시험시공계획
    • 부록C 반강성 포장 시험시공 현황 보고
    • 부록D 반강성 교면포장 시험시공 사진첩