    핵연료 피복관의 수소화합물 형성 및 파괴특성 = Mechaical Behavior:Hydride Formation and Failure Characteristics of Nuclear Fuel Cladding Tubes

    한글로보기

    https://www.riss.kr/link?id=A3235019

    • 0

      상세조회
    • 0

      다운로드
    서지정보 열기
    • 내보내기
    • 내책장담기
    • 공유하기
      • URL 복사
    • 오류접수
    인용문이 복사되었습니다.

    부가정보

    다국어 초록 (Multilingual Abstract) kakao i 다국어 번역

    The hydride formation characteristics and its effect on the failure mechanism of nuclear fuel claddings were investigated. The effect of cooling rate on the size, morphology and distribution of hydrides was also examined. Hydrides were more homogeneously distributed with high cooling rate (i.e, air-cooled) and clustered with low cooling rate (i.e, furnace-cooled). The room temperature strength increased slightly and the ductility decreased with hydrides formation. The size and distribution of hydrides were found to have insignificant effect on the mechanical properties. Secondary cracks along the platelets of hydrides were observed on the fracture surfaces of claddings fractured at low temperature. The loss of ductility at low temperature is thought to be associated with the cracking along the hydride platelets. Above 200℃, hydrides were dissolved during deformation and no secondary cracks were observed, suggesting that hydrides may not be detrimental to the high temperature ductility.
    번역하기

    The hydride formation characteristics and its effect on the failure mechanism of nuclear fuel claddings were investigated. The effect of cooling rate on the size, morphology and distribution of hydrides was also examined. Hydrides were more homogeneou...

    The hydride formation characteristics and its effect on the failure mechanism of nuclear fuel claddings were investigated. The effect of cooling rate on the size, morphology and distribution of hydrides was also examined. Hydrides were more homogeneously distributed with high cooling rate (i.e, air-cooled) and clustered with low cooling rate (i.e, furnace-cooled). The room temperature strength increased slightly and the ductility decreased with hydrides formation. The size and distribution of hydrides were found to have insignificant effect on the mechanical properties. Secondary cracks along the platelets of hydrides were observed on the fracture surfaces of claddings fractured at low temperature. The loss of ductility at low temperature is thought to be associated with the cracking along the hydride platelets. Above 200℃, hydrides were dissolved during deformation and no secondary cracks were observed, suggesting that hydrides may not be detrimental to the high temperature ductility.

    더보기

    목차 (Table of Contents)

    • 서론
    • 실험 방법
    • 결과 및 고찰
    • 수소화합물 형성
    • 수소화합물 형성에 따른 기계적 특성 및 파괴 특성
    • 서론
    • 실험 방법
    • 결과 및 고찰
    • 수소화합물 형성
    • 수소화합물 형성에 따른 기계적 특성 및 파괴 특성
    • 온도에 따른 파괴특성
    • 결론
    더보기

    동일학술지(권/호) 다른 논문

    동일학술지 더보기

    더보기

    분석정보

    View

    상세정보조회

    0

    Usage

    원문다운로드

    0

    대출신청

    0

    복사신청

    0

    EDDS신청

    0

    동일 주제 내 활용도 TOP

    더보기

    주제

    연도별 연구동향

    연도별 활용동향

    연관논문

    연구자 네트워크맵

    공동연구자 (7)

    유사연구자 (20) 활용도상위20명

    해외이동버튼