In order to synthesize the heat resistance ceramics of LAS system, we studied on preparing the fine powder with homogeneity by sol-gel method using metal alkoxide. Various results were obtained depending on the composition and process. When the amount...
In order to synthesize the heat resistance ceramics of LAS system, we studied on preparing the fine powder with homogeneity by sol-gel method using metal alkoxide. Various results were obtained depending on the composition and process. When the amount of H2O added at initial stage is higher than 10mol/$\ell$, and when the amount of catalyst is 0.1mol/$\ell$, the particle size of synthesized hydrate becomes finer. On condition that partial prehydrolysis time of TEOS is more than 50 hours, the monosized fine powder is obtained(below 1${\mu}{\textrm}{m}$).