The steelmaking dust treatment process has been established through reducing volatilization method in rotary kiln. The more content of zinc in reduced pellets and basicity of pellet is in the range of 1.5~3.0, the more working time needed in rotary ki...
The steelmaking dust treatment process has been established through reducing volatilization method in rotary kiln. The more content of zinc in reduced pellets and basicity of pellet is in the range of 1.5~3.0, the more working time needed in rotary kiln, because of decreasing wall accretion. A portion of well forming kiln coating in the furnace is a fourth of the total length from the outlet. Constitutes on the furnace wall accretion composed of the mixtures such as Fe, FeO, Fe₂O₃, Fe₃O₄, ZnO and CaO-SiO₂system, and formation of kiln coating is decreased by adding coke ratio.