CeO2–CuO catalyst prepared by citric acid method was investigated for selective catalytic reduction of NO with NH3. The activity of the CeO2 catalyst was enhanced about 8–27% in the temperature range of 125–225 ℃ at a space velocity of 28,000 ...
http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
https://www.riss.kr/link?id=A104707340
Rui-Tang Guo (Shanghai University of Electric Power) ; Wen-long Zhen (Shanghai University of Electric Power) ; Wei-Guo Pan (Shanghai University of Electric Power) ; Yue Zhou (Shanghai University of Electric Power) ; Jie-nan Hong (Shanghai University of Electric Power) ; Hong-jian Xu (Shanghai University of Electric Power) ; Qiang Jin (SEC-IHI Power Generation Environment Protection Engineering Co. Ltd.) ; Cheng-gang Ding (SEC-IHI Power Generation Environment Protection Engineering Co. Ltd.) ; Shi-yi Guo (SEC-IHI Power Generation Environment Protection Engineering Co. Ltd.)
2014
English
KCI등재,SCOPUS,SCIE
학술저널
1577-1580(4쪽)
73
0
상세조회0
다운로드다국어 초록 (Multilingual Abstract)
CeO2–CuO catalyst prepared by citric acid method was investigated for selective catalytic reduction of NO with NH3. The activity of the CeO2 catalyst was enhanced about 8–27% in the temperature range of 125–225 ℃ at a space velocity of 28,000 ...
CeO2–CuO catalyst prepared by citric acid method was investigated for selective catalytic reduction of NO with NH3. The activity of the CeO2 catalyst was enhanced about 8–27% in the temperature range of 125–225 ℃ at a space velocity of 28,000 h 1 by the addition of Cu. It was found that the state of Cu species had great impact on the SCR performance of CeO2–CuO catalyst. Cu2+ can enhance the low temperature activity of SCR reaction, while CuO would promote NH3 oxidation before SCR reaction at high temperature, which would cause the decrease of its high temperature SCR activity.
참고문헌 (Reference)
1 M. Moliner, 48 : 8264-8266, 2012
2 L. Wang, 289 : 21-29, 2012
3 M. H. Kim, 37 : 1333-1344, 2011
4 Z. Wu, 10 : 935-939, 2009
5 D. Liu, 93 : 194-204, 2009
6 X. Gao, 11 : 465-469, 2010
7 Y. Shen, 11 : 20-23, 2009
8 T. Gu, 12 : 310-313, 2010
9 L. Chen, 153 : 77-83, 2010
10 G. Qi, 39 : 848-849, 2003
1 M. Moliner, 48 : 8264-8266, 2012
2 L. Wang, 289 : 21-29, 2012
3 M. H. Kim, 37 : 1333-1344, 2011
4 Z. Wu, 10 : 935-939, 2009
5 D. Liu, 93 : 194-204, 2009
6 X. Gao, 11 : 465-469, 2010
7 Y. Shen, 11 : 20-23, 2009
8 T. Gu, 12 : 310-313, 2010
9 L. Chen, 153 : 77-83, 2010
10 G. Qi, 39 : 848-849, 2003
11 X. Gao, 12 : 255-258, 2010
12 X. Du, 270 : 370-376, 2013
13 X. Jiang, 34 : 591-598, 2013
14 B. Thirupathi, 110 : 195-206, 2011
15 D. Jiang, 17 : 59-63, 2012
16 G. Qi, 108 : 15738-15747, 2004
17 M. Mhamdi, 357 : 42-50, 2009
18 X. Du, 92 : 49-55, 2012
19 E. Y. Choi, 161 : 597-604, 1996
20 S. Damyanova, 234 : 271-282, 2002
21 B. Murugan, 112 : 20429-20442, 2008
22 X. Gao, 174 : 734-739, 2010
23 W. Shan, 115–116 : 100-106, 2012
24 G. Lu, 168 : 1128-1133, 2011
25 S. T. Korhonen, 47 : 800-802, 2011
26 J. Zhao, 52 : 1343-1353, 2011
Liquid permeability of packed bed with binary mixture of particles
학술지 이력
연월일 | 이력구분 | 이력상세 | 등재구분 |
---|---|---|---|
2023 | 평가예정 | 해외DB학술지평가 신청대상 (해외등재 학술지 평가) | |
2020-01-01 | 평가 | 등재학술지 유지 (해외등재 학술지 평가) | |
2011-01-01 | 평가 | 등재학술지 유지 (등재유지) | |
2009-01-01 | 평가 | 등재학술지 유지 (등재유지) | |
2007-01-01 | 평가 | 등재학술지 유지 (등재유지) | |
2004-01-01 | 평가 | 등재학술지 선정 (등재후보2차) | |
2003-01-01 | 평가 | 등재후보 1차 PASS (등재후보1차) | |
2001-07-01 | 평가 | 등재후보학술지 선정 (신규평가) |
학술지 인용정보
기준연도 | WOS-KCI 통합IF(2년) | KCIF(2년) | KCIF(3년) |
---|---|---|---|
2016 | 3.4 | 0.75 | 2.84 |
KCIF(4년) | KCIF(5년) | 중심성지수(3년) | 즉시성지수 |
2.39 | 2.24 | 0.397 | 0.56 |