High‑Efficiency Inhibition of Gravity Segregation in Al–Bi Immiscible Alloys by Adding Lanthanum
Peng Jia,Jinyang Zhang,Haoran Geng,Xinying Teng,Degang Zhao,Zhongxi Yang,Yi Wang,Song Hu,Jun Xiang,Xun Hu 대한금속·재료학회 2018 METALS AND MATERIALS International Vol.24 No.6
The inhibition of gravity segregation has been a long-standing challenge in fabrication and applications of homogeneousimmiscible alloys. Therefore, the effect of rare-earth La on the gravity segregation of Al–Bi immiscible alloys was investigatedto understand the homogenization mechanism. The results showed that the addition of La can completely suppress thegravity segregation. This is attributed to the nucleation of Bi-rich liquid phase on the in-situ produced LaBi2phase and thechange of the shape of LaBi2@Bi droplets. In addition, a novel strategy is developed to prepare the homogeneous immisciblealloys through the addition of rare-earth elements. This strategy not only is applicable to other immiscible alloys, but alsois conducive to finding more elements to suppress the gravity segregation. This study provided a useful reference for thefabrication of the homogeneous immiscible alloys.
Effect of Al on the Microstructure and Mechanical Properties of Mg–Sn–Ca–Mn Wrought Alloy
Yun Feng,Yuanyuan Yang,Zongqi Xiao,Xianglong Meng,Guorong Zhou,Jinfeng Leng,Xinying Teng 대한금속·재료학회 2022 METALS AND MATERIALS International Vol.28 No.6
Mg–Sn–Ca–Mn–xAl (x = 0,1.5 wt%) alloys with ultra-fine recrystallized grains were prepared by conventional extrusion(400 °C, 0.5 mm/s). Effects of aluminum (Al) on mechanical properties and microstructure of the Mg–1Sn–1Ca–0.5Mn(wt%) alloy were systematically investigated. By the addition of 1.5 wt% Al, the yield strength of the as-extruded alloysignificantly increased from 183 to 237 MPa. The as-cast alloys show a dendritic structure consists of α-Mg, (Mg, Al)2Ca,and CaMgSn phases. The as-extruded Mg–1Sn–1Ca–0.5Mn–1.5Al alloys exhibit a bimodal grain structure composed ofdynamic recrystallized (DRXed) fine grains and coarse unDRXed grains. Compared with Al free alloy, a lot of nano-scaleplanar Al2Caand rectangle shape Al8Mn5precipitated in the as-extruded alloy with 1.5 wt% Al. Meanwhile, the addition ofAl significantly strengthened alloys’ fiber texture with < 10–10 >//ED.