송종법(Jong-Beop Song),최일경(Il-kyung Choi),정효경(Hyo-kyung Jung),권순홍(Soon-Hong Kwon),권순구(Soon-Gu Kwon),박종민(Jong-Min Park),김종순(Jong-Soon Kim),정성원(Sung-Won Jung),최원식(Won-Sik Choi) 한국산업융합학회 2017 한국산업융합학회 논문집 Vol.20 No.2
Dental implants are required to have biomechanical functions and biostability in order to perform authoring, pronunciation, and aesthetic functions in the oral cavity. In terms of biostability, pure titanium for medical have good biostability and no rejection in the alveolar bone. with appropriate strength in terms of strength as well as biocompatibility. In recent years, various surgical methods and devices have been developed to improve the convenience and safety of the procedure. However, as the number of procedures increases, the screw loosening of the abutment screw connecting the artificial root and the abutment There are many reports of artificial root and abutment fracture. Fig. 1 is an example of a case where the upper part of the abutment screw is arbitrarily modified to remove the abutment by the abutment fracture due to the loosening of the abutment screw. The fundamental cause of abduction of the abutment screw is caused by the slight movement due to the lowering of the retention force of the abutment screw. It is necessary to minimize loosening of the abutment screw to avoid problems such as fracture during the period of using the implant. The purpose of this study is to investigate the structure of the abutment screw to prevent the loosening of the abutment screw by forming 0.5mm slot
마이크로 아크 산화 표면처리 기술을 활용한 치과도재 소부용 티타늄 인공치아 결합강도 연구
송종법 ( Jong-beop Song ),박종민 ( Jong-min Park ),김종순 ( Jong-soon Kim ),정효경 ( Hyo-kyung Jung ),최원식 ( Won-sik Choi ) 한국산업융합학회 2022 한국산업융합학회 논문집 Vol.25 No.2
The bonding strength [ISO22674] test was conducted by firing a dedicated ceramic powder on the surface of the dental titanium material treated with micro-arc oxidation. In the test group, an average result value of 34.34 MPa was obtained, and in the control group, a result value of 21.53 MPa was obtained. The bonding strength of the test group was higher than that of the control group by 12.81 MPa, resul ting in a 37% improvement in durability of the dental artificial tooth ceramic restoration.