http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
Uzay Koc-Vural,Ismail Baltacioglu,Pinar Altinci 대한치과보존학회 2017 Restorative Dentistry & Endodontics Vol.42 No.2
Objectives: This study aimed to evaluate the color stability of bulk-fill and nanohybrid resin-based composites polished with 3 different, multistep, aluminum-oxide impregnated finishing and polishing disks. Materials and Methods: Disk-shaped specimens (8 mm in diameter and 4 mm in thickness) were light-cured between two glass slabs using one nanohybid bulk-fill (Tetric EvoCeram, Ivoclar Vivadent), one micro-hybrid bulk-fill (Quixfil, Dentsply), and two nanohybrid incremental-fill (Filtek Ultimate, 3M ESPE; Herculite XRV Ultra, Kerr) resin-based composites, and aged by thermocycling (between 5 - 55°C, 3,000 cycles). Then, they were divided into subgroups according to the polishing procedure as SwissFlex (Coltène/Whaledent), Optidisc (Kerr), and Praxis TDV (TDV Dental) (n = 12 per subgroup). One surface of each specimen was left unpolished. All specimens were immersed in coffee solution at 37°C. The color differences (ΔE) were measured after 1 and 7 days of storage using a colorimeter based on CIE Lab system. The data were analyzed by univariate ANOVA, Mann-Whitney U test, and Friedmann tests (α = 0.05). Results: Univariate ANOVA detected significant interactions between polishing procedure and composite resin and polishing procedure and storage time (p < 0.05). Significant color changes were detected after 1 day storage in coffee solution (p < 0.05), except Quixfil/Optidisc which was color-stable after 7 days (p > 0.05). Polishing reduced the discoloration resistance of Tetric EvoCeram/SwissFlex, Tetric EvoCeram/Praxis TDV, Quixfil-SwissFlex, and all Herculite XRV Ultra groups after 7 days storage (p < 0.05). Conclusions: Discoloration resistance of bulk-fill resin-based composites can be significantly affected by the polishing procedures.
Comparison of two different methods of detecting residual caries
Vural, Uzay Koc,Kutuk, Zeynep Bilge,Ergin, Esra,Cakir, Filiz Yalcin,Gurgan, Sevil The Korean Academy of Conservative Dentistry 2017 Restorative Dentistry & Endodontics Vol.42 No.1
Objectives: The aim of this study was to investigate the ability of the fluorescence-aided caries excavation (FACE) device to detect residual caries by comparing conventional methods in vivo. Materials and Methods: A total of 301 females and 202 males with carious teeth participated in this study. The cavity preparations were done by grade 4 (Group 1, 154 teeth), grade 5 (Group 2, 176 teeth), and postgraduate (Group 3, 173 teeth) students. After caries excavation using a handpiece and hand instruments, the presence of residual caries was evaluated by 2 investigators who were previously calibrated for visual-tactile assessment with and without magnifying glasses and trained in the use of a FACE device. The tooth number, cavity type, and presence or absence of residual caries were recorded. The data were analyzed using the Chi-square test, the Fisher's Exact test, or the McNemar test as appropriate. Kappa statistics was used for calibration. In all tests, the level of significance was set at p = 0.05. Results: Almost half of the cavities prepared were Class II (Class I, 20.9%; Class II, 48.9%; Class III, 20.1%; Class IV, 3.4%; Class V, 6.8%). Higher numbers of cavities left with caries were observed in Groups 1 and 2 than in Group 3 for all examination methods. Significant differences were found between visual inspection with or without magnifying glasses and inspection with a FACE device for all groups (p < 0.001). More residual caries were detected through inspection with a FACE device (46.5%) than through either visual inspection (31.8%) or inspection with a magnifying glass (37.6%). Conclusions: Within the limitations of this study, the FACE device may be an effective method for the detection of residual caries.
Koc-Vural, Uzay,Baltacioglu, Ismail,Altinci, Pinar The Korean Academy of Conservative Dentistry 2017 Restorative Dentistry & Endodontics Vol.42 No.2
Objectives: This study aimed to evaluate the color stability of bulk-fill and nanohybrid resin-based composites polished with 3 different, multistep, aluminum-oxide impregnated finishing and polishing disks. Materials and Methods: Disk-shaped specimens (8 mm in diameter and 4 mm in thickness) were light-cured between two glass slabs using one nanohybid bulk-fill (Tetric EvoCeram, Ivoclar Vivadent), one micro-hybrid bulk-fill (Quixfil, Dentsply), and two nanohybrid incremental-fill (Filtek Ultimate, 3M ESPE; Herculite XRV Ultra, Kerr) resin-based composites, and aged by thermocycling (between $5-55^{\circ}C$, 3,000 cycles). Then, they were divided into subgroups according to the polishing procedure as SwissFlex ($Colt\grave{e}ne/Whaledent$), Optidisc (Kerr), and Praxis TDV (TDV Dental) (n = 12 per subgroup). One surface of each specimen was left unpolished. All specimens were immersed in coffee solution at $37^{\circ}C$. The color differences (${\Delta}E$) were measured after 1 and 7 days of storage using a colorimeter based on CIE Lab system. The data were analyzed by univariate ANOVA, Mann-Whitney U test, and Friedmann tests (${\alpha}=0.05$). Results: Univariate ANOVA detected significant interactions between polishing procedure and composite resin and polishing procedure and storage time (p < 0.05). Significant color changes were detected after 1 day storage in coffee solution (p < 0.05), except Quixfil/Optidisc which was color-stable after 7 days (p > 0.05). Polishing reduced the discoloration resistance of Tetric EvoCeram/SwissFlex, Tetric EvoCeram/Praxis TDV, Quixfil-SwissFlex, and all Herculite XRV Ultra groups after 7 days storage (p < 0.05). Conclusions: Discoloration resistance of bulk-fill resin-based composites can be significantly affected by the polishing procedures.