Sakon Sansongsiri,Somchai Thongtem 한양대학교 세라믹연구소 2016 Journal of Ceramic Processing Research Vol.17 No.12
Titanium dioxide (TiO2) thin films were deposited on glass substrates by filtered cathodic vacuum arc system (lab-made) forvarious number of pulse modes at -50 VDC, and followed by 450 oC annealing in air for 1 hr. The deposition pulses were 500-2,000 pulses and the anatase film thickness was 13.0-37.5 nm. In this research, the roughness was increased with the increasingin the number of deposition pulses and film thickness. The transmission at 600 nm wavelength was 65-85%, decreasing withthe film thickness, and the optical energy gap was in the range of 3.55-3.65 eV