( Ismail Kirbas ),( Alper Karahan ),( Abdullah Sevin ),( Cuneyt Bayilmis ) 한국인터넷정보학회 2013 KSII Transactions on Internet and Information Syst Vol.7 No.8
Recently, the use of wireless body area networks (WBAN) has been increasing rapidly in medical healthcare applications. WBANs consist of smart nodes that can be used to sense and transmit vital data such as heart rate, temperature and ECG from a human body to a medical centre. WBANs depend on limited resources such as energy and bandwidth. In order to utilise these resources efficiently, a very well organized medium access control (MAC) protocol must be considered. In this paper, a new, adaptive and energy-efficient MAC protocol, entitled isMAC, is proposed for WBANs. The proposed MAC is based on multi-channel communication and aims to prolong the network lifetime by effectively employing (i) a collision prevention mechanism, (ii) a coordinator node (WCN) selection algorithm and (iii) a transmission power adjustment approach. The isMAC protocol has been developed and modelled, by using OPNET Modeler simulation software. It is based on a networking scenario that requires especially high data rates such as ECG, for performance evaluation purposes. Packet delay, network throughput and energy consumption have been chosen as performance metrics. The comparison between the simulation results of isMAC and classical IEEE 802.15.4 (ZigBee) protocol shows that isMAC significantly outperforms IEEE 802.15.4 in terms of packet delay, throughput and energy consumption.
The effect of repeated porcelain firings on corrosion resistance of different dental alloys
Ali Riza Tuncdemir,Ismail Karahan,Serdar Polat,Meral Arslan Malkoc,Mehmet Dalkiz 대한치과보철학회 2013 The Journal of Advanced Prosthodontics Vol.5 No.1
PURPOSE. The aim of this study was to evaluate the effects of repeated porcelain firing process on the corrosion rates of the dental alloys. MATERIALS AND METHODS. Cr-Co, Cr-Ni and Pd-Ag alloys were used for this study. Each metal supported porcelain consisted of 30 specimens of 10 for 7, 9 and 11 firing each. Disc-shaped specimens 10 mm diameter and 3 mm thickness were formed by melting alloys with a propane-oxygen flame and casted with a centrifuge casting machine and then with the porcelain veneer fired onto the metal alloys. Corrosion tests were performed in quintuplicate for each alloy (after repeated porcelain firing) in Fusayama artificial saliva solution (pH = 5) in a low thermal-expansion borosilicate glass cell. Tamhane and Sheffe test was used to compare corrosion differences in the results after repeated firings and among 7, 9 and 11 firing for each alloy. The probability level for statistical significance was set at α=0.05. RESULTS. The corrosion resistance was higher (30 mV), in case of 7 times firing (Commercial). On the other hand, it was lower in case of 11 times firing (5 mV) (P<.05). Conclusion. Repeated firings decreased corrosion resistance of Pd-Ag, Cr-Co and Cr-Ni alloys. The Pd-Ag alloy exhibited little corrosion in in vitro tests. The Cr-Ni alloy exhibited higher corrosion resistance than Cr-Co alloys in in vitro tests.