http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
Influence of different universal adhesives on the repair performance of hybrid CAD-CAM materials
Demirel, Gulbike,Baltacioglu, Ismail Hakki The Korean Academy of Conservative Dentistry 2019 Restorative Dentistry & Endodontics Vol.44 No.3
Objectives: The aim of this study was to investigate the microshear bond strength (${\mu}SBS$) of different universal adhesive systems applied to hybrid computer-aided design/computer-aided manufacturing (CAD-CAM) restorative materials repaired with a composite resin. Materials and Methods: Four types of CAD-CAM hybrid block materials-Lava Ultimate (LA), Vita Enamic (VE), CeraSmart (CS), and Shofu Block HC (SH)-were used in this study, in combination with the following four adhesive protocols: 1) control: porcelain primer + total etch adhesive (CO), 2) Single Bond Universal (SB), 3) All Bond Universal (AB), and 4) Clearfil Universal Bond (CU). The ${\mu}SBS$ of the composite resin (Clearfil Majesty Esthetic) was measured and the data were analyzed using two-way analysis of variance and the Tukey test, with the level of significance set at p < 0.05. Results: The CAD-CAM block type and block-adhesive combination had significant effects on the bond strength values (p < 0.05). Significant differences were found between the following pairs of groups: VE/CO and VE/AB, CS/CO and CS/AB, VE/CU and CS/CU, and VE/AB and CS/AB (p < 0.05). Conclusions: The ${\mu}SBS$ values were affected by hybrid block type. All tested universal adhesive treatments can be used as an alternative to the control treatment for repair, except the AB system on VE blocks (the VE/AB group). The ${\mu}SBS$ values showed variation across different adhesive treatments on different hybrid CAD-CAM block types.
Uzay Koc-Vural,Ismail Baltacioglu,Pinar Altinci 대한치과보존학회 2017 Restorative Dentistry & Endodontics Vol.42 No.2
Objectives: This study aimed to evaluate the color stability of bulk-fill and nanohybrid resin-based composites polished with 3 different, multistep, aluminum-oxide impregnated finishing and polishing disks. Materials and Methods: Disk-shaped specimens (8 mm in diameter and 4 mm in thickness) were light-cured between two glass slabs using one nanohybid bulk-fill (Tetric EvoCeram, Ivoclar Vivadent), one micro-hybrid bulk-fill (Quixfil, Dentsply), and two nanohybrid incremental-fill (Filtek Ultimate, 3M ESPE; Herculite XRV Ultra, Kerr) resin-based composites, and aged by thermocycling (between 5 - 55°C, 3,000 cycles). Then, they were divided into subgroups according to the polishing procedure as SwissFlex (Coltène/Whaledent), Optidisc (Kerr), and Praxis TDV (TDV Dental) (n = 12 per subgroup). One surface of each specimen was left unpolished. All specimens were immersed in coffee solution at 37°C. The color differences (ΔE) were measured after 1 and 7 days of storage using a colorimeter based on CIE Lab system. The data were analyzed by univariate ANOVA, Mann-Whitney U test, and Friedmann tests (α = 0.05). Results: Univariate ANOVA detected significant interactions between polishing procedure and composite resin and polishing procedure and storage time (p < 0.05). Significant color changes were detected after 1 day storage in coffee solution (p < 0.05), except Quixfil/Optidisc which was color-stable after 7 days (p > 0.05). Polishing reduced the discoloration resistance of Tetric EvoCeram/SwissFlex, Tetric EvoCeram/Praxis TDV, Quixfil-SwissFlex, and all Herculite XRV Ultra groups after 7 days storage (p < 0.05). Conclusions: Discoloration resistance of bulk-fill resin-based composites can be significantly affected by the polishing procedures.
Koc-Vural, Uzay,Baltacioglu, Ismail,Altinci, Pinar The Korean Academy of Conservative Dentistry 2017 Restorative Dentistry & Endodontics Vol.42 No.2
Objectives: This study aimed to evaluate the color stability of bulk-fill and nanohybrid resin-based composites polished with 3 different, multistep, aluminum-oxide impregnated finishing and polishing disks. Materials and Methods: Disk-shaped specimens (8 mm in diameter and 4 mm in thickness) were light-cured between two glass slabs using one nanohybid bulk-fill (Tetric EvoCeram, Ivoclar Vivadent), one micro-hybrid bulk-fill (Quixfil, Dentsply), and two nanohybrid incremental-fill (Filtek Ultimate, 3M ESPE; Herculite XRV Ultra, Kerr) resin-based composites, and aged by thermocycling (between $5-55^{\circ}C$, 3,000 cycles). Then, they were divided into subgroups according to the polishing procedure as SwissFlex ($Colt\grave{e}ne/Whaledent$), Optidisc (Kerr), and Praxis TDV (TDV Dental) (n = 12 per subgroup). One surface of each specimen was left unpolished. All specimens were immersed in coffee solution at $37^{\circ}C$. The color differences (${\Delta}E$) were measured after 1 and 7 days of storage using a colorimeter based on CIE Lab system. The data were analyzed by univariate ANOVA, Mann-Whitney U test, and Friedmann tests (${\alpha}=0.05$). Results: Univariate ANOVA detected significant interactions between polishing procedure and composite resin and polishing procedure and storage time (p < 0.05). Significant color changes were detected after 1 day storage in coffee solution (p < 0.05), except Quixfil/Optidisc which was color-stable after 7 days (p > 0.05). Polishing reduced the discoloration resistance of Tetric EvoCeram/SwissFlex, Tetric EvoCeram/Praxis TDV, Quixfil-SwissFlex, and all Herculite XRV Ultra groups after 7 days storage (p < 0.05). Conclusions: Discoloration resistance of bulk-fill resin-based composites can be significantly affected by the polishing procedures.