석탄비산재로부터 합성한 제올라이트를 이용한 유가금속이온의 흡착속도 및 등온 해석
안갑환 ( Kab-hwan Ahn ),이창한 ( Chang-han Lee ),이민규 ( Min-gyu Lee ) 한국환경과학회 2018 한국환경과학회지 Vol.27 No.2
In this study, zeolite (Z-C2) was synthesized using a fusion/hydrothermal method on coal fly ash (FA) discharged from a thermal power plant in the Ulsan area and then analyzed via scanning electron microscopy (SEM) and X-ray diffraction (XRD). The Z-C2 was characterized in terms of mineralogical composition and morphological analysis. The XRD results showed that its peaks had the characteristics of Na-A zeolite in the range of 2θ of 7.18~34.18. The SEM images confirmed that the Na-A zeolite crystals had a chamfered-edge crystal structure almost identical to that of the commercial zeolite. The adsorption kinetics of Cu, Co, Mn and Zn ions by Z-C2 were described better by the pseudo-second-order kinetic model more than by the pseudo-first-order kinetic model. The Langmuir model fitted the adsorption isotherm data better than the Freundlich model did. The maximum adsorption capacities of Cu, Co, Mn and Zn ions obtained from the Langmuir model were in the following order : Cu (94.7 mg/g) > Co (77.7 mg/g) > Mn (57.6 mg/g) > Zn (51.1 mg/g). These adsorption capacities are regarded as excellent compared to those of commercial zeolite.
상수원수의 혼화 및 응집 조건에 따른 DAF pump 장치의 부상분리효율
안갑환 ( Kab Hwan Ahn ),이창한 ( Chang Han Lee ) 한국환경과학회 2011 한국환경과학회지 Vol.20 No.5
This study found that flotation efficiencies for removing algae and micro particles in raw water were optimized on mixing intensity and time of the mixing and flocculation conditions with a continuous DAF system. It is more efficient for mixing intensity at 23.1 s-1 and time at 660 s(Gt value: 15246) to float flocculated floc with the raw water in M water treatment plant. Flotation efficiency was more than about 0.9 when operated pressure and A/S ratio were sustained at 5 kgf·cm-2 and up to 0.056 mL·mg-1. The continuous DAF system made by the study could be continuously operated for 20 days and sustained not exceeding 4 NTU with raw water with low turbidity(13.4~9.8 NTU).
비틀대모자반, Sargassum sagamianum을 이용한 Pb 및 Cr 생체흡착 및 회수
서근학,안갑환,이학성,이회근,조진구,홍용기,SUH Kuen-Hack,AHN Kab-Hwan,LEE Hack-Sung,LEE Hwae-Geon,CHO Jin-Koo,HONG Yong-Ki 한국수산과학회 1999 한국수산과학회지 Vol.32 No.4
우리나라 인근 해역에서 가장 쉽게 채취할 수 있는 해조류 중의 하나인 S. sagamianum을 이용한 Pb 및 Cr의 생체흡착 실험을 수행하였다. Pb 및 Cr은 15분 안에 흡착 평형에 도달하였으며, 평형흡착량은 각각 224.5mg Pb/g biomass 및 77.5mg Cr/g bio-mass로서 Pb의 흡착량이 Cr보다 약 3배정도 높았다. 또한 pH가 감소할수록 Pb 및 Cr의 홉착량은 감소하였으나 Pb가 상대적으로 많은 영향을 받는 것으로 나타났다. Pb, Cr, Cu 및 Cd 혼합용액에서는 Pb>Cu>Cr>Cd 순으로 흡착하였으며, Pb 및 Cr 이온이동량 존재하는 용액에서의 흡착은 거의 1 : 1로 흡착이 이루어졌다. Pb 및 Cr흡착 후에 0.1 M HCl, 0.1 M $HNO_3$ 및 0.1 M EDTA으로 탈착 실험을 수행하니, Pb는 의 경우에는 $95\%$이상 탈착되었으나 Cr의 경우 S. sagamianum와의 결합력이 상대적으로 강하여 탈착율이 $51\%$이하로 낮았다. Biosorption of Pb and Cr to Sargassum sagamianum was evaluated in the various conditions. An adsorption equilibrium was reached in about 15 min. for Pb and Cr. The uptake capacity was 224.5 mg Pb/g biomass and 77.5 mg Cr/g biomass, respectively. The adsorption parameters for Pb and Cr were determined according to Langmuir and Freundlich model. Biosorption of Pb and Cr was increased with an increase in pH value. Pb and Cr adsorbed by S. sagamianum could be recovered by desorption process with 0.1M HCl, 0.1M $HNO_3$ and 0.1M EDTA and the efficiency of Pb desorption was above $90\%$, whereas the efficiency of Cr desorption was below $51\%$.
Dewatering Characteristics for Physico-chemical Properties with Sewage Sludge
이창한,안갑환,송승구,Lee, Chang-Han,Ahn, Kab-Hwan,Song, Seung-Koo The Korean Society for Biotechnology and Bioengine 2010 KSBB Journal Vol.8 No.1
In this study, we found that dewatering properties were related with physico-chemical properties such as sludge concentration, pH, and zeta potential with sewage sludge, Ionic contents in digested sludge were in the order of $Ca^{2+}$ (14.2 mg/g) > $Mg^{2+}$ (1.9 mg/g) > $Na^+$ (1.4 mg/g) > $K^+$ (1.0 mg/g). Divalent ion more than monovalent have influenced on physico-chemical and dewatering properties. Floc size distribution in activated (AS) and digested sludge (DS) increased on lower pH range to be near isoelectric point and than specific resistance to filtration (SRF) decreased. A linear increase in SRF ($5.25\times10^{13}\sim2.86\times10^{14}$ m/kg in AS and $6.89\times10^{14}\sim1.09\times10^{15}$ m/kg in DS) was observed throughout low concentration range of 1230~9960 mg/L in AS and 2700~5400 mg/L in DS.
괭생이모자반, Sargassum horneri를 이용한 Pb 흡착 및 탈착
서근학,안갑환,김병진,조진구,진형주,홍용기,SUH Kuen-Hack,AHN Kab-Hwan,KIM Byong-Jin,CHO Jin-Koo,JIN Hyung-Joo,HONH Yong-Ki 한국수산과학회 1999 한국수산과학회지 Vol.32 No.3
우리나라 인근 해역에서 가장 쉽게 채취할 수 있는 해조류중의 하나인 S. horneri을 이용한 Pb 의 생체흡착 실험을 수행하였다. 흡착 평형에는 15분 안에 도달하였으며, 평형흡착량은 185.5mg Pb/g biomass 이었다. pH가 감소할수록 Pb는 흡착량이 현저히 감소하였다. 또한 Pb 흡착시에 Ca 및 Mg가 500mg/L 존재하여도 Ca 및 Mg 등의 경금속은 전혀 흡착되지 않고 Pb만을 선택적으로 제거하는 것이 가능하였으나, 고농도로 존재하는 경금속들이 inhibotor 작용을 하여 Pb의 흡착량은 다소 감소하였다. Pb흡착 및 탈착 과정을 6회 반복한 결과, HCl 및 $HNO_3$ 이용한 경우에 흡착된 Pb의 회수 및 S. horneri의 재생에 있어 매우 효과적인 것으로 나타났다. Biosorption of Pb to Sargassum horneri was evaluated. An adsorption equilibrium was reached in about 15 min. for Pb and Pb uptake was 185.5 mg Pb/g biomass. When Ca and Mg concentration increases in Pb solution, Pb was selectively adsorbed. The Pb adsorbed by S. horneri could be recovered by desorption process, and the desorption efficiency of Pb by 0.1 M HCl, 0.1 M $HNO_3$, and 0.1 M EDTA was above $95\%$, whereas the elution by 0.1 M NaOH was less efficient in the desorption of Pb. S. horneri was reused 6 cycle repeatedly after adsorption/desorption and the sum of uptake was 636.6 mg Pb/g biomass.