This paper described the changes of peel strength, wrinkle recovery and dimensional stability after fusing 4 different wool face fabrics with 3 different fusible interlinings. The fusing condition was conducted by fusing press machine under 4kg·f/cm^...
This paper described the changes of peel strength, wrinkle recovery and dimensional stability after fusing 4 different wool face fabrics with 3 different fusible interlinings. The fusing condition was conducted by fusing press machine under 4kg·f/cm^2 at 150℃.
To determine the effect of the various physical properties of the fused fabrics, face fabrics and interlinings on the peel strength, wrinkle recovery and dimensional stability(hygral expansion and relaxation shrinkage) of fused fabrics, correlation among the KES values of fused fabrics of fused fabrics, face fabrics and interlinings to the peel strength, wrinkle recovery and dimensional stability of fused fabrics were experimentally analyzed.
As the results, the peel strength was mainly influenced by the cover factor of face fabric and interlinings.
After fusing wrinkle recovery and hygral expansion were decreased. The cover factor, wrinkle recovery, weight, thickness, shear rigidity and frictional properties of face fabric, and the thickness of fused fabrics were highly correlated with the wrinkle recovery of fused fabrics. But the physical properties of the interlinings did not influence to the wrinkle recovery of fused fabrics.
In addition, the dimensional stabilities of fused fabrics were mainly influenced by the tensile and frictional properties of the face fabrics.