    SCOPUS KCI등재 SCIE

    연소합성법에 의한 Plasma-arc Deposit 용 $Cr_3C_2$ 합성 및 특성에 관한 연구 = Synthesis and Characterization of $Cr_3C_2$ for Plasma-arc Deposit by Combustion Synthesis Process

    한글로보기

    https://www.riss.kr/link?id=A106127506

    • 0

      상세조회
    • 0

      다운로드
    서지정보 열기
    • 내보내기
    • 내책장담기
    • 공유하기
    • 오류접수
    인용문이 복사되었습니다.

    부가정보

    다국어 초록 (Multilingual Abstract) kakao i 다국어 번역

    Using Cr2O3 Al and graphite powders as starting materials Cr3C2 was synthesized by combustion synthesis process according to the following reaction : 3Cr3C2 +4C+6Allongrightarrow2Cr3C2 +3Al2O3. The synthesis was conducted at 2 atm in an argon atmosphere. in this study main-product was monolithic phase of Cr3C2 /Cr7C3 mixture and sub-product was slag state of $\alpha$-Al2O3. Single phase of Cr3C2 was obtained when crushed main-product was heat-treated at 120$0^{\circ}C$ for 3h in vacuum state with addition of 2.5wt% C. The obtained Cr3C2 powder can be used as plasma-arc deposit material because the flowability index of powder with the size of 9-50${\mu}{\textrm}{m}$ was 66.
    번역하기

    Using Cr2O3 Al and graphite powders as starting materials Cr3C2 was synthesized by combustion synthesis process according to the following reaction : 3Cr3C2 +4C+6Allongrightarrow2Cr3C2 +3Al2O3. The synthesis was conducted at 2 atm in an argon atmosphe...

    Using Cr2O3 Al and graphite powders as starting materials Cr3C2 was synthesized by combustion synthesis process according to the following reaction : 3Cr3C2 +4C+6Allongrightarrow2Cr3C2 +3Al2O3. The synthesis was conducted at 2 atm in an argon atmosphere. in this study main-product was monolithic phase of Cr3C2 /Cr7C3 mixture and sub-product was slag state of $\alpha$-Al2O3. Single phase of Cr3C2 was obtained when crushed main-product was heat-treated at 120$0^{\circ}C$ for 3h in vacuum state with addition of 2.5wt% C. The obtained Cr3C2 powder can be used as plasma-arc deposit material because the flowability index of powder with the size of 9-50${\mu}{\textrm}{m}$ was 66.

    더보기

    동일학술지(권/호) 다른 논문

    분석정보

    View

    상세정보조회

    0

    Usage

    원문다운로드

    0

    대출신청

    0

    복사신청

    0

    EDDS신청

    0

    동일 주제 내 활용도 TOP

    더보기

    주제

    연도별 연구동향

    연도별 활용동향

    연관논문

    연구자 네트워크맵

    공동연구자 (7)

    유사연구자 (20) 활용도상위20명

    이 자료와 함께 이용한 RISS 자료

    나만을 위한 추천자료

    해외이동버튼